Wang Zhu-bo,Jie Chen,Rutie Liu,Hao Li,Xueyang Lin,Da He,Xiang Xiong
标识
DOI:10.1016/j.apt.2020.06.030
摘要
This paper explored a solid-phase reduction method to prepare ultrafine nickel powder under different conditions. The effect of a NaCl separator agent on the morphology, primary particle size and specific surface area of the prepared nickel powder is discussed. The results show that direct contact among primary Ni particles can be effectively inhibited during the reduction of nickel oxalate due to the presence of the NaCl separator agent. An ultrafine nickel powder with a primary particle size of between 80 and 150 nm can be prepared with NaCl as the separator agent at temperatures from 400 °C to 460 °C. The powder reduced at 430 °C has a uniform particle distribution and a decreased amount of agglomeration.