摘要
Dendrite growth, corrosion, passivation, and other side reactions during Zn plating and stripping have consistently hindered the capacity and lifespan of Zn metal batteries. In this study, we employ first-principles calculations to unravel the epitaxial electroplating mechanism of Zn (002) planes on various substrate surfaces. We identify six critical factors, including interfacial stability, zincophilicity, surface atomic arrangement, lattice mismatch, responsiveness, and adaptability, that profoundly influence the electrochemical behavior of zinc deposition. Our findings reveal that substrates with hexagonal surface atomic arrangements and strong metallic bonding with zinc, such as (002)-Zn, (111)-Cu, and Ti
科研通智能强力驱动
Strongly Powered by AbleSci AI