Young Ji Park,Jong Hyeok LEE,Younki Lee,Tae Wook Kang,Sun Woog Kim
标识
DOI:10.1016/j.rineng.2026.114044
摘要
Achieving dense oxide-based solid electrolytes with sufficient ionic conductivities typically requires high-temperature sintering, which remains a major processing challenge. Glass-based sintering additives have been shown to effectively lower sintering temperature. We investigated the effects of 40Li 2 O-40B 2 O 3 -(20-x)SiO 2 -xGeO 2 (LBSG) (5 ≤ x ≤ 15) glass prepared via melt quenching on the sintering behavior of Li 1.3 Al 0.3 Ti 1.7 (PO 4 ) 3 (LATP), a suitable solid-state electrolyte for lithium-ion batteries. Among the investigated LBSG compositions, LBSG (x = 10) glass was identified as the optimal sintering additive and was thereafter incorporated into LATP to fabricate LATP–LBSG composites containing 1–9 wt% LBSG. Specifically, LATP–5 wt% LBSG sintered at a much lower temperature of 650 °C for 30 min and showed an ionic conductivity of 6.6 × 10 ⁻6 S cm -1 , comparable to that of the LATP reference sintered at 900 °C for 2 h. After warm isostatic pressing, the ionic conductivity of this composite increased significantly to 1.15 × 10 ⁻5 S cm -1 . Further, to evaluate the applicability of this low-temperature-processed electrolyte in battery applications, a coin-type cell, with Li metal as the anode and LiCoO 2 as the cathode (Li/LATP-5 wt% LBSG/LiCoO 2 ), was fabricated. This cell showed an initial discharge capacity of 98.99 mAh g -1 at 0.1 C, which remained high at 89.85 mAh g -1 even after five cycles, indicating that it retained 90.87% of its initial capacity. Overall, LBSG glass additives can help to retain the conductivity of LATP at the reference level, enabling sintering under substantially reduced temperatures and processing times.
科研通智能强力驱动
Strongly Powered by AbleSci AI