S. Seema,T. Thangesh,R. Anuradha,Rajasekaran T.R,Dr. S. K. Nagarajan,V. Sabarinathan
标识
DOI:10.62441/nano-ntp.v20is8.111
摘要
Membrane durability is one of the critical issues in the development of proton exchange membrane fuel cells (PEMFC). In this paper, the authors studied effects of aging on various solvents such as ethanol, isopropyl alcohol (IPA) and distilled water (DM) based on its proton conductivity using electrochemical impedance spectroscopy (EIS). Further, the swelling nature is reported along with its structural properties and transport mechanism. A facile non-conducting (medium) homemade setup under an aqueous environment used to study conductivity. Nafion 117 membrane is being a perfluoro sulfonated ionomer to be very sensitive under aging treatment when it was stored for very long period at 36 ⁰C (humid atmospheres). Moreover, the aging process inducing the condensation of sulfonic groups to form anhydrides as interpreted. Highest ionic conductivity of 0.069 x 10-1 S cm-1 was observed on first day in DM water which is higher than in that of ethanol and IPA solvents. This conductivity value in water occurs with respect to its pH level and seems to be strong evidence for better performance in PEM fuel cells.
科研通智能强力驱动
Strongly Powered by AbleSci AI