The effective work function (EWF) of WN x C y on SiO 2 /Si stacks can be modulated from 4.3 to 4.8 eV by plasma-enhanced atomic layer deposition. At higher annealing temperature, more oxidation of WN x C y near SiO 2 can yield larger dipole with the direction from thin interfacial WN x C y :O to bulk WN x C y , and thus EWF increases. WN 0.12 C 0.23 with lower nitrogen content captures more oxygen atoms in the interfacial WN x C y from SiO 2 than WN 0.39 C 0.1 and yields larger work function. Using different thicknesses of top WN 0.12 C 0.23 and bottom WN 0.39 C 0.1 with constant total thickness, the EWF can be tuned by dipole strength at WN 0.39 C 0.1 /WN x C y :O interface. The dipole-controlled WN x C y work function metal is integrated on the stacked GeSn nanosheets (NSs) to achieve multi- ${V}_{T}$ modulation. ${V}_{T}$ for stacked Ge 0.87 Sn 0.13 NSs is increasingly negative with increasing WN 0.39 C 0.1 thickness with a wide ${V}_{T}$ tunability of 510 mV.