箔法
锂(药物)
材料科学
腐蚀
电解质
溶解
降级(电信)
阴极
相对湿度
电极
铝
化学工程
分析化学(期刊)
化学
冶金
复合材料
环境化学
医学
电信
物理
物理化学
计算机科学
工程类
热力学
内分泌学
作者
Thomas Langner,Tim Sieber,Anja Rietig,Virginia Merk,Lutz Pfeifer,Jörg Acker
标识
DOI:10.1038/s41598-023-32688-0
摘要
Abstract The present study deals with the phenomenological observation of the corrosion of the positive electrode foil of lithium-ion batteries containing LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC) as cathode material. Due to the presence of moisture, localized water accumulation is formed on the NMC surface. The water absorbed by the electrolyte reacts with the NMC under Li + /H + exchange and the resulting pH increase leads to dissolution of the carrier foil and characteristic salt-like blooms on the NMC surface. With the increase in the relative area occupied by the holes in the aluminum foil per time, a sufficiently suitable parameter was found with which to quantitatively determine the extent of corrosion. The degree of degradation depends on time and ambient humidity. It was shown that functional recycling with the water jet method is no longer applicable for degraded foils, since the mechanical stability of the foils decreases as corrosion progresses. Lithium, aluminum, sulfur and oxygen were detected in the blooms using SEM–EDX and Laser-Induced-Breakdown-Spectroscopy (LIBS). The underlying NMC layer was found to contain mainly aluminum and significantly lower lithium content than the non-degraded material. SEM and Raman microscopy analyses also showed that the active material is also locally degraded and therefore no longer suitable for functional recycling.
科研通智能强力驱动
Strongly Powered by AbleSci AI