摘要
An impurity phase, Na 3 MnO 4 , is often overlooked during the synthesis of Mn-based sodium layered oxides due to its absence in X-ray diffraction (XRD) patterns, leading to misjudged phase purity and overestimated Na/TM ratios in the targeted materials. In this work, we confirmed its presence through titration and elemental analysis and showed its profound influence on the electrochemical responses. We proposed that Na 3 MnO 4 , formed at elevated temperatures, rapidly degrades in ambient air because of its highly hygroscopic nature and reactivity with water, rendering it “invisible” to XRD. Remarkably, incorporating 2 at.% Ca not only improves the air stability of the host materials but also stabilizes the Na 3 MnO 4 impurity phase, making it detectable by XRD. This simple yet effective strategy is applicable to various Mn-based sodium layered oxides and offers new insights into their phase purity and accurate Na/TM ratio.
科研通智能强力驱动
Strongly Powered by AbleSci AI