Lithium ion-sieve of λ-MnO2 was prepared by leaching precursor LiMn2O4 in 0.5 mol/L HCl solution to remove Li+,the Li+ exchange capacity of Li+ sieve at different pH values and its adsorption kinetics were studied,and some samples were also characterized by XRD and SEM.The results indicate that some nuances appear in the microstructure of the samples after adsorbing lithium ion,but it is still similar to LiMn2O4.The longer the time of elution,the higher the elution ratio of Li+ on the adsorbent;simultaneously,the adsorbent dissolving ratio of manganese also increases.The extraction ratio of Li+ from LiMn2O4 is 97% and the dissolving ratio of Mn2+ is 15% after 5 h leaching.The exchange capacity of the ion-sieve is enhanced with the increase of pH in the process of adsorption and its balance adsorption capacity is 23.75 mg/g when pH is 12.95 in LiOH solution.The adsorption process is found to fit pseudo-second-order kinetic equation and the Langmuir isotherm equation,so the adsorption process is determined to be chemical adsorption and monolayer adsorption.