腐蚀
熔盐
共晶体系
氯化物
材料科学
高温腐蚀
冶金
热能储存
极化(电化学)
合金
化学
生物
生态学
物理化学
作者
Ángel G. Fernández,Luisa F. Cabeza
标识
DOI:10.1016/j.est.2019.101125
摘要
The operating temperature of a steam turbine is limited to 565 ºC by the molten nitrate heat-transfer fluid; therefore, a new molten salt chemistry is needed to increase the maximum operating temperature in the new generation of CSP plants and improve the thermal-to-electrical energy conversion efficiency in the turbine block, such as chloride molten salts. Nevertheless, the prevention of high-temperature corrosion on containment materials using chlorides plays a critical role and a corrosion mitigation plan is needed to achieve the target plant lifetime of 30 years. This paper presents a corrosion mitigation strategy focused on different thermal treatments performed in the eutectic ternary chloride molten salt composed by MgCl 2 /NaCl/KCl (55.1 wt.%/24.5 wt.%/20.4 wt.%). Corrosion rates were obtained through linear polarization resistance technique in a conventional commercial stainless steel (AISI 304) at 720 ºC during 5 h of immersion after the different thermal treatments carried out. Scanning electron microscopy and XRD analysis were used to confirm the corrosion rates and corrosion layer proposed by electrochemical techniques, obtaining a minimum corrosion rate of 6.033 mm/year for the best thermal treatment performed.
科研通智能强力驱动
Strongly Powered by AbleSci AI