This paper studies the preparation of dialdehyde cellulose (DAC).The influences of the reaction temperature,the solution pH value,the oxidizing agent concentration,the reaction time,and their interactions on the aldedyde content of DAC were discussed by orthogonal experiment when using NaIO_4 as the oxidizing agent.So the most principal factors that affect the aldedyde content of DAC were the reaction temperature.the interaction of the reaction temperature and the NaIO_4 concentration,and the interaction of the reaction temperature and the solution pH value.The oxidation conditions were optimized.When the reaction temperature was 35℃,the reaction time was 3h,the NaIO_4 concentration was 6.78%,the pH was 2,and the aldehyde content of DAC was 68.20%.