BaMoO4 ceramic was prepared using a conventional solid-sintering method. It was observed that the sample is a pure BaMoO4 with a tetragonal scheelite structure by analyzing X-ray diffraction data. Scanning electron microscopy characterized the dense sample with uniform grains. The phonon modes were analyzed by Raman and Far-infrared reflection spectra, and the phonon characteristics were studied. The intrinsic properties of the sample were calculated by the four-parameter semi-quantum model as well as the Clausius-Mosotti & damping equations, and the results were of εr = 9.388 and tanδ = 4.760 × 10−4, εr = 9.798 and tanδ = 6.445 × 10−4, respectively, which agrees well with the experimental values (εr = 9.84, tanδ = 5.0 × 10−4). The contributions to dielectric properties of each mode were investigated, and the results indicate that the external mode (Eu) yield greatest contribution to intrinsic permittivity and loss.