MoSi 2 doped Yb 2 Si 2 O 7 composites were designed to extend the lifetime of Yb 2 Si 2 O 7 environmental barrier coatings (EBCs) via self-healing cracks during high-temperature applications. Yb 2 Si 2 O 7 –Yb 2 SiO 5 –MoSi 2 composites with different mass fractions were prepared by applying spark plasma sintering. X-ray diffraction results confirmed that the composites consisted of Yb 2 Si 2 O 7 , Yb 2 SiO 5 , and MoSi 2 . The thermal expansion coefficients (CTEs) of the composites increased with an increase in the MoSi 2 content. The average CTE of the 15 wt% MoSi 2 doped Yb 2 Si 2 O 7 composite was 5.24 × 10 −6 K −1 , indicating that it still meets the CTE requirement of EBC materials. After being pre-cracked by using the Vickers indentation technique, the samples were annealed for 0.5 h at 1100 or 1300 °C to evaluate the crack-healing ability. Microstructural studies showed that cracks in 15 wt% MoSi 2 doped Yb 2 Si 2 O 7 composites were fully healed during annealing at 1300 °C. Two mechanisms may be responsible for crack healing. First, the cracks were filled with SiO 2 glass formed by MoSi 2 oxidation. Second, the formed SiO 2 continued to react with Yb 2 SiO 5 to form Yb 2 Si 2 O 7 , which can cause cracks to heal owing to volumetric expansion. The Yb 2 Si 2 O 7 formation with smaller volume expansion is more beneficial.
科研通智能强力驱动
Strongly Powered by AbleSci AI