期刊:Advances in transdisciplinary engineering [IOS Press] 日期:2025-10-10
标识
DOI:10.3233/atde250994
摘要
In this study, an Al-5.0Mg-2.0Zn-1.0Ce-0.5Mn-0.2Sc (wt.%) alloy was designed and subjected to different heat treatment regimens to investigate the effects of various elements on the alloy’s microstructure, room-temperature properties, and high-temperature stability. The results indicate that the as-cast matrix contained multiple secondary phases formed during solidification: Al11Ce3, Al3Sc, Mn-rich, and T(AlMgZn) phases. Following ageing treatment, the T phase dissolved into the matrix, while the other secondary phases remained observable. Transmission electron microscopy (TEM) revealed the precipitation of Al3Sc phases after ageing. Specifically, the two-step ageing treatment (300°C/5h + 400°C/3h) yielded the maximum volume fraction and density of nano-sized Al3Sc precipitates. Additionally, rod-shaped T(AlMgZn) phase precipitates were observed after the three-step ageing treatment (300°C/5h + 400°C/3h + 140°C/14h). In mechanical property testing, the alloy subjected to the double-step ageing treatment exhibited the optimal properties, achieving a room-temperature tensile strength of 294 MPa. However, its strength decreased after thermal exposure at 300°C for 100 hours. This decline is due to the substantial precipitation of Mg and Zn, leading to the formation of coarse secondary phases. Despite this decrease, the strength remained relatively high at 273 MPa. This retention of strength is attributed to the excellent coarsening resistance of the Al11Ce3, Al3Sc, and Mn-rich phases. We designed a heat-resistant aluminum alloy incorporating three distinct strengthening mechanisms that work synergistically, offering a novel approach for developing new heat-resistant aluminum alloys.