摘要
The additional graphitisation required to produce high-modulus PAN-based carbon fibres comes at the expense of their compression strength. Consequently, this study re-evaluates the assumption that the conditions for mesoscale instability are met before the fibre strength is reached. Four fibre grades are evaluated: T700S (230 GPa), T800S (294 GPa), M40J (377 GPa), and M46J (436 GPa). Laminates share the same epoxy matrix, stacking sequence, and manufacturing process. Coupons are tested in compression (ASTM D6641) and four-point bending (ASTM D6272). The through-thickness strain gradient in flexure, which delays mesoscale instability, is used to infer the failure mechanism, supported by post-mortem fracture morphology, mechanism-based analytical modelling, and reported fibre strengths. The difference in failure strain between methods diminishes from 42% (T700S) and 62% (T800S) to 17% (M40J) and -6% (M46J); compression fracture morphology shifts from brooming to planar between T800S and M40J; mesoscale instability models, accurate within 5% for T700S and T800S, overpredicted by 34% and 52% for M40J and M46J; and back-calculated fibre stresses indicate that the M40J and M46J laminates fail near their fibre strengths. This evidence supports a transition from mesoscale instability of the composite to fibre strength-controlled failure in laminates reinforced with the M40J and M46J fibre grades.
科研通智能强力驱动
Strongly Powered by AbleSci AI