Dasom Kim,Akihiro Choshi,Yuhki Tsukada,Naoki Takata
标识
DOI:10.1016/j.addma.2025.105035
摘要
This study was undertaken to address dominant microstructural factors in the melt-pool structure formed in powder bed fusion using laser beam (PBF-LB) for high strength and the mechanical behavior of Al-2.5 %Fe binary alloy samples additive-manufactured via PBF-LB. Single-crystal micropillars with a mean diameter of approximately 2 μm were fabricated at different regions of the melt-pool structure (melt-pool inside: MPI, melt-pool boundary: MPB), and compression tests were performed at various initial strain rates controlled by loading rate. The PBF-LB process produced numerous Al 6 Fe metastable phases (with a few tens of nanometers in size) distributed in the α-Al supersaturated solid solutions containing highly concentrated Fe in a large part of the melt-pool inside (MPI). A relatively coarsened microstructure with a thickness of approximately 3 µm (composed of many granular α-Al phase with a few hundred nanometer size surrounded by Al 6 Fe-phase particles) was localized at the melt-pool boundary (MPB) region. The MPI micropillars exhibited a higher 0.2 % proof stress than the MPB micropillars, whereas the following strain hardening appeared similar due to the activation of multiple slip systems. The MPI micropillars exhibit almost the same mechanical behavior after the 300 ℃ annealing for the formation of nanoscale precipitates consuming solute Fe, indicating that the refined Al 6 Fe phase is a dominant contributor to the strengthening by the PBF-LB process. Intriguingly, MPI micropillars exhibited a negative strain rate sensitivity of flow stress at an early stage of deformation, whereas the negative strain rate sensitivity transitioned to positive after annealing at 300 ℃. TEM characterization revealed the dynamic precipitation of nanoscale Fe-rich precipitates inside the α-Al(fcc) matrix with high solute Fe contents even at ambient temperature. The nanoscale precipitates interact with introduced dislocations, resulting in the enhanced flow stress at an early stage of plastic deformation. The present study provided new insights into a local variation in strain-rate dependent strength depending on the location of the melt pool structure in Al alloys processed via PBF-LB, in terms of solute alloy-element contents (driving force for the dynamic precipitation) controlled by laser conditions of the PBF-LB process.
科研通智能强力驱动
Strongly Powered by AbleSci AI