Makoto Hasegawa,Akira Isogai,Fumihiko Onabe
标识
DOI:10.1016/0144-8617(93)90100-i
摘要
Two types of low degree of polymerisation (DP) chitosan were prepared by homogeneous hydrolysis of chitosan in 85% phosphoric acid at room temperature for 1–6 weeks. The hydrolysates were collected by addition of excess ethanol, and were fractionated by solubility in water. The changes in yields of water-insoluble (higher DP) and water-soluble (lower DP) fractions were determined as a function of hydrolysis time. The hydrolysis proceeded with further deacetylation of chitosan, resulting in degree of deacetylation of more than 90%. The water-insoluble fraction prepared after the hydrolysis for 4 weeks (43% yield) had a weight-average DP (DPw) of 16·8, and showed the 'tendon' type X-ray diffraction pattern. The water-soluble fraction (12·5% yield) had a DPw of 7·3, and showed the 'annealed' type pattern.
科研通智能强力驱动
Strongly Powered by AbleSci AI