Enbo Yang,Joshua M. Grant,Alexander Golden,Joe Margetis,Wei Du,Shui-Qing Yu
标识
DOI:10.1149/2162-8777/adcc4f
摘要
Abstract GeSn alloy has gained significant attention for its compatibility with Si photonics platforms and its engineerable bandgap covering mid-infrared (MIR) wavelengths. Chemical vapor deposition (CVD) is widely used to synthesize GeSn materials. However, a fundamental understanding of the growth mechanism must still be developed. This research used mass spectrometry to investigate CVD gas phase reactions at various temperatures of 25°C, 100°C, 150°C, and 200°C for a gas mixture of GeH4 and SnCl4 with various gas partial pressure ratios (pSnCl4 /pGeH4 ) of 0.002, 0.005, 0.01 and 0.042. The analysis of the experimental results indicates two types of gas phase reactions occurred in all scenarios examined. The reactions involve direct interactions between SnCl4 and GeH4, as well as the decomposition of GeH4. The hybrid radicals of Sn, H3SnCl/SnCl, the Germanium hybrid fragments of H3GeCl/GeCl, H2GeCl2/GeCl2, and GeHx and hydrogens (H, H2, and H3+) are the primary products of the first and second types of reactions, respectively. These reactions exhibit increased reactivity at higher temperatures, and the resulting intermediates are essential for the GeSn CVD process. Density functional theory-based thermochemical calculations agree with the experimental results and indicate that the proposed chemical reactions are either exothermic or minimally endothermic.
科研通智能强力驱动
Strongly Powered by AbleSci AI