Toshitaka Tanabe,Yasutaka Nagai,Takeshi Hirabayashi,Nobuyuki Takagi,Kazuhiko Dohmae,Naoki Takahashi,Shinichi Matsumoto,Hirohumi Shinjoh,Junko N. Kondo,J.C. Schouten,Hidde H. Brongersma
标识
DOI:10.1016/j.apcata.2009.09.030
摘要
Unexpectedly large amounts of CO adsorption have resulted from a pulse adsorption experiment at 323 K, giving about 300% Pt dispersion in a Pt/cerium-based oxide catalyst. An in situ diffuse reflectance infrared Fourier transform spectroscopic investigation on a Pt/cerium-based oxide during CO adsorption has revealed that carbonate species on the cerium oxide surface are responsible for the unrealistically large CO adsorption at 323 K, as a result of CO spillover. Lowering the temperature to 195 K considerably diminished the amount of CO adsorption. The size of the Pt particles in the Pt/cerium-based oxide catalyst was determined by CO pulse adsorption at 195 K and showed good agreement with the particle size determined by X-ray diffraction and low energy ion scattering. This indicates that CO pulse adsorption at 195 K is a useful technique to reliably estimate the Pt particle size in a Pt/cerium-based oxide catalyst.
科研通智能强力驱动
Strongly Powered by AbleSci AI