Ziwei Ye,Libin Zhang,Hussein Hijazi,Ben Tang,Yixiang Zhang,Svena Yu,Haoqi Ni,Bailey Rutherford,Jeff R. Dahn,Michael Metzger
标识
DOI:10.1149/1945-7111/ae2f2e
摘要
The O3-type sodium layered oxide NaMO 2 , where M is a mix of Mn, Fe, Ni and Zn, here NaMn 0.39 Fe 0.31 Ni 0.22 Zn 0.08 O 2 , has a specific capacity of ∼140 mAh g −1 when charged to 4.0 V, highlighting its potential as a positive electrode material for sodium-ion batteries. Electrochemical tests on machine-made pouch cells indicate that increasing the upper cut-off voltage from 3.8 to 3.9 V and 4.0 V leads to initially higher capacity which fades rapidly over cycling. Isothermal microcalorimetry, ultra-high precision coulometry and micro-X-ray fluorescence spectroscopy ruled out parasitic reactions between the electrolyte and the partially de-sodiated positive electrode surface as a major contributing factor to the inferior electrochemical performance at 4.0 V. Instead, it was found by ex situ and in situ X-ray diffraction that repeated cycling to 4.0 V induces the formation of an octahedral/prismatic hybrid phase, which leads to a collapse of the c lattice parameter in the crystal structure, resulting in poor long-term reversibility and ultimately poor cycle life. This irreversible structure transformation is the primary mechanism for poor cycling stability of the O3-type sodium layered oxide NaMO 2 at high voltage.
科研通智能强力驱动
Strongly Powered by AbleSci AI