作者
Yu-Yi Ye,José Almeida Gonilha,Nuno M. Silvestre,João R. Correia
摘要
This paper investigates the transverse compressive translaminar fracture behavior of pultruded glass fiber reinforced polymer (GFRP) materials at elevated temperature. Compact compression (CC) tests were conducted at room temperature (∼18 °C) and three constant elevated temperatures (40 °C, 60 °C, and 80 °C). Failure modes and load-displacement curves were analyzed. Damage evolution parameters, including transverse compressive fracture toughness ( ) and residual strength ( ), were calibrated by fitting finite element (FE) predictions to experimental curves, using a trilinear damage evolution law combined with the Hashin failure criteria. The effects of elevated temperature on these parameters were examined, and was compared with the corresponding tensile fracture toughness ( ). Results indicate that, for the range of temperatures tested, although increasing temperature reduces stiffness and peak load, the compressive fracture behavior exhibits a gradual softening response that is largely temperature-independent. decreases with increasing temperature, with retention values of 0.895, 0.846, and 0.585 at 40 °C, 60 °C, and 80 °C, respectively, whereas presents an almost horizontal plateau, with corresponding relative increases of 22.7%, 13.0%, and 18.7%. Furthermore, is comparable to at lower temperatures but exceeds at higher temperatures. In addition, exhibits a clear exponential dependence on the transverse tensile strength ( ) across all temperatures, whereas remains uncorrelated with the transverse compressive strength ( ) at room temperature, but increases proportionally with at elevated temperature.