摘要
In this work, we focus on the degradation of membrane electrode assemblies (MEAs) in proton-exchange membrane water electrolysis (PEMWE) induced by different accelerated stress tests (ASTs), including constant-current mode, square-wave mode, and solar photovoltaic mode. In constant-current mode, at continuous testing for 600 h at 80 °C, a degradation of operating voltage increased by the enhanced current density from 22 µV/h (1 A/cm2) to 50 µV/h (3 A/cm2). In square-wave mode, we found that in the narrow fluctuation range (1–2 A/cm2), the shorter step time (2 s) generates a higher degradation rate of operating voltage, but in the wide fluctuation range (1–3 A/cm2), the longer step time (22 s) induces a faster operating voltage rise. In the solar photovoltaic mode, we used a simulation of 11 h sunshine duration containing multiple constant-current and square-wave modes, which is closest to the actual application environment. Over 1400 h ASTs, the solar photovoltaic mode lead to the most serious voltage rise of 87.7 µV/h. These results are beneficial to understanding the durability of the PEM electrolyzer and optimizing the components of MEAs, such as catalysts, membranes, and gas diffusion layers.
科研通智能强力驱动
Strongly Powered by AbleSci AI