摘要
Aluminum sheets were immersed in CuCl₂ solution for different periods and then kept at 150 °C for 20 h. SEM and XRD observations were used to compare the surfaces obtained under the different conditions. Their wetting behavior and corrosion response were examined by contact-angle, EIS, and polarization measurements. The specimen etched for 20 s gave the highest contact angle, 152°, while its sliding angle was approximately 8°. Compared with bare aluminum, this specimen produced a larger impedance arc and a lower corrosion current density. The inhibition efficiency calculated from the EIS fitting parameters was 26.88%. Following 2400 abrasion cycles, the contact angle fell to 123°. The worn surface was still hydrophobic, although it no longer retained the original superhydrophobic state. Thus, the combination of CuCl₂ etching and heating improved the corrosion response without requiring a separate low-surface-energy treatment.
科研通智能强力驱动
Strongly Powered by AbleSci AI