材料科学
夏比冲击试验
因科镍合金
液化
冶金
Laves相
电子束焊接
高温合金
焊接
微观结构
焊接性
合金
阴极射线
金属间化合物
电子
物理
量子力学
作者
Hyun-Uk Hong,Sang-Hyun Bae,Soon-Il Kwon,Je-Hyun Lee,Jeonghyeon Do,Baig-Gyu Choi,In-Soo Kim,Chang-Yong Jo
标识
DOI:10.5781/kwjs.2013.31.6.50
摘要
Characterization of microstructures and cryogenic mechanical properties of electro beam (EB) welds between cast and forged Inconel 718 superalloys has been investigated. Optimal EBW condition was found in the beam current range of 36~39 mA with the constant travel speed of 12 mm/s and arc voltage of 120 kV for 10 mm-thick specimens. Electron beam current lower than 25 mA caused to occur the liquation microfissuring in cast-side heat affected zone (HAZ) of EB welds. The HAZ liquation microfissure was found on the liquated grain boundaries with resolidified ${\gamma}/Laves$ and ${\gamma}/NbC$ eutectic constituents. EBW produced welds showing a fine dendritic structure with relatively discrete Laves phase due to fast cooling rate. After post weld aging treatment, blocky Laves phase and formation of ${\gamma}^{\prime}+{\gamma}^{{\prime}{\prime}}$ strengtheners were observed. Presence of primary strengthener and coarse Laves particles in PWHT weld may cause to reduce micro-plastic zone ahead of a crack, leading to a significant decrease in Charpy impact toughness at $-196^{\circ}C$ . Fracture initiation and propagation induced by Charpy impact testing were discussed in terms of the dislocation structures ahead of crack arisen from the fractured Laves phase.
科研通智能强力驱动
Strongly Powered by AbleSci AI