摘要
The SUS321H and SUS347H steel tubes, extensively used as superheaters and reheaters in fossil fuel-fired power plant boilers, were subjected to long term steam oxidation tests for up to 3.6×107 s (10000 h) to clarify the steam oxidation behavior.It was revealed that the scales formed on the both steel tubes exposed in the steam of 848∼923 K for 1.08×106∼3.6×107 s are composed of an outer scale (Fe3O4) and an inner scale ((Fe, Cr, Ni)3O4), and that their thickness ratio is 45:55. When the boundary between the inner scale and the substrate metal reaches to a grain boundary of the original metal, a Cr-rich oxide layer is formed there. The Cr rich oxide layer protects the metal from oxidation. Thus, the growth of the inner scale does not obey the parabolic oxidation law. The inner scale thickness, di, can be expressed as a function of time, t, by the following equation.(This article is not displayable. Please see full text pdf.) \ oindentwhere kE is a function of temperature and α is a function of grain size.
科研通智能强力驱动
Strongly Powered by AbleSci AI