Rojee Oh,Jung-Hwa Lim,Chan-Gyu Lee,Keun-Woo Lee,Sung Yong Kim,Jong-Eun Kim
标识
DOI:10.1016/j.jmbbm.2023.105906
摘要
The use of digital manufacturing, particularly additive manufacturing using three-dimensional (3D) printing, is expanding in the field of dentistry. 3D-printed resin appliances must undergo an essential process, post-washing, to remove residual monomers; however, the effect of the washing solution temperature on the biocompatibility and mechanical properties remains unclear. Therefore, we processed 3D-printed resin samples under different post-washing temperatures (without temperature control (N/T), 30 °C, 40 °C, and 50 °C) for different durations (5, 10, 15, 30, and 60 min) and evaluated the degree of conversion rate, cell viability, flexural strength, and Vickers hardness. Increasing the washing solution temperature significantly improved the degree of conversion rate and cell viability. Conversely, increasing the solution temperature and time decreased the flexural strength and microhardness. This study confirmed that the washing temperature and time influence the mechanical and biological properties of the 3D-printed resin. Washing 3D-printed resin at 30 °C for 30 min was most efficient to maintain optimal biocompatibility and minimize changes of mechanical properties.
科研通智能强力驱动
Strongly Powered by AbleSci AI