尖晶石
溶解
材料科学
微观结构
相(物质)
断裂韧性
韧性
矿物学
冶金
化学工程
复合材料
化学
有机化学
工程类
作者
Jesse Miller,Ivar E. Reimanis,Marc Rubat du Merac
摘要
Abstract Dissolution of Al 2 O 3 particles into a MgAl 2 O 4 (spinel) matrix is accompanied by a volumetric expansion that is predicted to lead to a compressive stress field upon cooling, resulting in a promising microstructure for enhanced toughening of transparent spinel. This study explores the conditions to form such a microstructure by hot‐pressing powders of Al 2 O 3 and spinel, at temperatures that promote dissolution of the Al 2 O 3 . Tough, particulate‐reinforced composites were formed under lower temperatures and shorter times, but single phase, cubic spinel was formed at 1700°C for 10 hours. The single phase spinel made in this way exhibited a toughness of 2.26 ± 0.17 MPa√m, significantly higher than the equivalent nonstoichiometric spinel made by traditional methods, 1.72 ± 0.06 MP a√m. X‐ray diffraction measurements revealed lattice parameter changes consistent with the dissolution of Al 2 O 3 into spinel. Mechanics modeling reveals that toughening arises due to the volume expansion as Al 2 O 3 dissolves into the spinel matrix.
科研通智能强力驱动
Strongly Powered by AbleSci AI