Xiao Hui Wang,Yanchun Zhou
标识
DOI:10.1007/s10019-003-0252-4
摘要
Ti3AIC2 has good oxidation resistance at high temperatures owing to the formation of protective Al2O3 layer. However, as it is directly exposed to air at 500 °C and especially 600 °C, the scales formed on Ti3AIC2 exhibits poor protectivity because of the oxidation-induced microcracks, which limits the potential application of this technologically important material. In this work, the oxidation resistance of Ti3AIC2 at 500 °C and 600 °C was significantly improved by pre-oxidation at 1000–1300 °C for a short time of 2 h in air. The oxidation of the pre-oxidized Ti3AIC2 at 600 °C generally obeyed a parabolic rate law instead of the speed-up linear relation in the case without pre-oxidation. As revealed by X-ray diffraction, Raman spectroscopy results and SEM observations, the remarkable improvement of oxidation resistance after pre-oxidation was attributed to the protective layers formed on Ti3AIC2 during pre-oxidation, which inhibited the formation of anatase TiO2 that resulted in the oxidation-induced microcracks. Moreover, this work confirmed that the mechanism proposed previously for the anomalous oxidation of Ti3AIC2 in air at 500–600 °C was correct.
科研通智能强力驱动
Strongly Powered by AbleSci AI