Tao Xiang,Fan Zhang,Chao Yin
出处
期刊:Advanced Materials Research
[Trans Tech Publications]
日期:2012-09-01
卷期号:568: 52-56
被引量:5
标识
DOI:10.4028/www.scientific.net/amr.568.52
摘要
A phosphoru-nitrogen intumescent flame retardant (SCF101) consisting of acid source, carbon source and gas source, was synthesized by phosphoric acid, phosphorus pentoxide, pentaerythritol and melamine (MA). TGA and SEM results showed that decomposition temperature range of SCF101 was from 100°C to 700°C, and the residual char yield ratio was 30-40%, and the char layer was uniform and compact. As a substitute of traditional flame retardant, namely, ammonium polyphosphate (APP), melamine (MA) and pentaerythritol (PER), the SCF101 used in fireproof coatings of steel structure can improve residual char yield about 10%. The gasoline blowtorch experiments showed that the foam expansion of the coating containing SCF101 was higher, and char layer structure was compact and continuous, while the coating containing APP, MA and PER can not foam uniformly and the foam was cracked under the action of flame.
科研通智能强力驱动
Strongly Powered by AbleSci AI