摘要
The original Superpave low-temperature specification for asphalt binders placed limits on the low-temperature stiffness and m-value. A recently approved alternative to the original Superpave asphalt binder low-temperature specification makes use of the measured stiffness and tensile strength of the binder to determine a critical cracking temperature. Thermal cracking temperatures are presented for 42 plain and modified asphalt binders. Thermal cracking temperatures determined by the original and recently approved alternative Superpave specification are compared. The fracture toughness, K IC , can also be used to evaluate low-temperature cracking properties of asphalt binders. Fracture properties obtained for 14 asphalt binders are compared with the thermal cracking temperatures determined by the original and recently adopted alternative Superpave specifications. The set of 14 binders was produced from a common base material but modified by different means. For the set of 14 binders, there is little difference in their ranking according to both the original and recently proposed alternative Superpave low-temperature criteria; however, their ranking is quite different on the basis of the fracture properties as measured by K IC . K IC appears to provide a much more discriminating ranking of the binders than either of the Superpave specification criteria.
科研通智能强力驱动
Strongly Powered by AbleSci AI