Abstract We investigate the thickness dependence of the passivation quality of silicon nitride (SiN x ) films formed by catalytic chemical vapor deposition. The passivation quality of SiN x films, evaluated by measuring effective minority carrier lifetime ( τ eff ), can be enhanced by post annealing, and show a significant thickness dependence. τ eff increases with SiN x thickness up to 90 nm and shows no more significant improvement with further increase in SiN x thickness. Interface state density ( D it ) shows high consistency with thickness dependence of τ eff before and after annealing, whereas fixed charge density ( Q f ) rather decreases with increase in SiN x thickness. We propose a possible mechanism that SiN x films may release hydrogen (H) atoms during post annealing to terminate dangling bonds on the c-Si surface which leads to decrease in D it . Increase of τ eff with SiN x thickness before annealing might be caused by the annealing effect from a heated catalyzing wire.