木质素磺酸盐
化学
硬木
软木
大小排阻色谱法
摩尔质量分布
色谱法
分析化学(期刊)
特性粘度
木质素
植物
有机化学
聚合物
酶
生物
作者
Svein Magne Braaten,Bjørn E. Christensen,Guro Elise Fredheim
标识
DOI:10.1081/wct-120021925
摘要
Abstract Lignosulfonates obtained from spruce (Picea abies), aspen (Populus sp.) and two species of Eucalyptus (E. globulus and E. grandis) were characterized by aqueous size exclusion chromatography (SEC) combined with in-line multi-angle laser light scattering (MALLS). In general, the hardwood lignosulfonates were shifted to lower molecular weights (M w = 5.700–12.000 g/mol) as compared to softwood lignosulfonates (M w = 36.000–61.000 g/mol). Lignosulfonates from E. grandis were further fractionated to obtain fractions of different molecular weights (3.500–30.000 g/mol). The degree of sulfonation increased with decreasing M w for the fractions as previously found for fractions of spruce lignosulfonate (Fredheim, G.; Braaten S.M.; Christensen, B.E. Molecular weight determination of lignosulfonates by size exclusion chromatography and multi-angle laser lightscattering. J. Chromatogr. 2002, 942, 191–199). The relationship between the intrinsic viscosity (in 0.1 M NaCl) and molecular weight was essentially the same for spruce and E. grandis lignosulfonate fractions, with an estimated Mark–Houwink–Sakurada (MHS) exponent of 0.36. This value, combined with the low intrinsic viscosities, confirms that lignosulfonates are compact structures in aqueous solution. Based on the SEC–MALLS results a SEC-method using a UV-detector (SEC–UV) was developed, where lignosulfonate fractions were used as broad molecular weight calibration standards. Keywords: LignosulfonateHardwoodSoftwoodLight scatteringMolecular weightMolecular weight distribution Acknowledgments We gratefully acknowledge technical and economical support from Borregaard LignoTech, Norway. The authors wish to thank research Director Trond Rojahn for valuable discussions. Ms. Pham thi thuy Hong is thanked for skillful technical assistance.
科研通智能强力驱动
Strongly Powered by AbleSci AI