作者
Andrew Guy Thomas,Wendy R. Flavell,A. K. Mallick,Asurasinghe R. Kumarasinghe,Dimitra Tsoutsou,Nasir Khan,C. Chatwin,Sarah Rayner,Graham C. Smith,Roger Stockbauer,Samantha Warren,T. K. Johal,S. Patel,David M. P. Holland,Amina Taleb-Ibrahimi,Frédéric Wiame
标识
DOI:10.1103/physrevb.75.035105
摘要
A comparison of the electronic structure of rutile (110), anatase (101), and anatase (001) single-crystal surfaces has been made using resonant photoemission and x-ray absorption spectroscopy. Under identical preparative conditions, the anatase (101) surface shows the lowest $\mathrm{Ti}\phantom{\rule{0.3em}{0ex}}3d$ and $4sp$ hybridization in the states close to the valence-band maximum of the three surfaces. It also shows the highest concentration of surface-oxygen vacancies. The effect on the electronic structure of modifying the surface preparative route and thus the concentration of surface-oxygen vacancies is examined. The $\ensuremath{\sigma}$-antibonding $\mathrm{Ti}\phantom{\rule{0.3em}{0ex}}3d\phantom{\rule{0.3em}{0ex}}{e}_{g}∕\mathrm{O}\phantom{\rule{0.3em}{0ex}}2p$ hybridization (probed by XAS) is reduced by the removal of surface-oxygen. Photoemission shows that as the number of surface-defects is increased, the $\mathrm{O}\phantom{\rule{0.3em}{0ex}}2p\text{\ensuremath{-}}\mathrm{Ti}\phantom{\rule{0.3em}{0ex}}3d\phantom{\rule{0.3em}{0ex}}{t}_{2g}\phantom{\rule{0.3em}{0ex}}\ensuremath{\pi}$-bonding interaction is disrupted. For the anatase (101) surface it is found that as the number of surface-oxygen vacancies is increased, the $\mathrm{Ti}\phantom{\rule{0.3em}{0ex}}3d$ and $4sp$ contributions at the valence-band maximum are reduced. We discuss the correlation between electronic structure and photocatalytic activity of the different polymorphs of ${\mathrm{TiO}}_{2}$.
科研通智能强力驱动
Strongly Powered by AbleSci AI