Synthesis and Electrochemical Performance Studies of LiMn_(2-x-y-z)Tl_xAl_yM_zO_4 (M=Co, Cr and Ni) Cathode Materials for Lithium Ion Secondary Batteries
The complex LiMn2-x-y-zTlxAlyMzO4(M=Co, Cr and Ni) cathode materials with spinel type structure were synthesized by co doping Tl, Al and M atoms at the same time and using improved solid state reaction, and their physical and electrochemical properties were investigated by XRD, SEM, TEM, CV and electrochemical testing. The electrochemical performances of as synthesized cathode materials at 25℃ and 55℃ were studied and measured. The results demonstrated that the as synthesized cathode materials have complete spinel structure the same as parent LiMn2O4 spinel, the samples have uniform morphology and normal grain size distribution. When M is Co and Cr, the mean size of the resulted samples is 800nm, and the initial charge capacity of LiMn1.90Tl0.05Al0.02M0.03O4 cathode materials was 123.70mAh·g-1 and 121.30mAh·g-1, respectively, and the discharge capacity of LiMn1.90Tl0.05Al0.02M0.03O4 is 117.30mAh·g-1 and 115.70mAh·g-1, respectively. Whereas M is Ni, the result of the corresponding cathode material is poor, the initial charge and discharge capacity is only 109.20mAh·g-1 and 99.78mAh·g-1. The cathode material has two charge and discharge plateaus in the course of charge and discharge respectively when M is Co, Cr or/and Ni. The two plateaus have the tendency of gradually becoming into only one plateau with the increase of lithium dopant amount. When M is Co or/and Cr, the resulted cathode materials have excellent room temperature (25℃) and higher temperature (55℃) performances, which can be attributed to the synergistic interaction between these metals, the synergistic interaction increases the stability of the cathode materials. These properties make the cathode materials become the promising cathode materials and widely applied in the future electric vehicles(EV) and hybrid electric vehicles(HEV) batteries.