摘要
Prussian blue and its analogs (PB/PBAs) have an open three-dimensional structure that allows for the facile insertion and extraction of sodium ions, making them promising candidates for cathode materials in sodium-ion batteries (SIBs). PB/PBAs also offers cost advantages, as it uses inexpensive iron and forms crystals in solution simplifying the synthesis process. Unlike other layered cathode materials, which require high-temperature sintering, PB/PBAs can be synthesized via precursor mixing or self-assembly in acidic conditions, thereby reducing energy consumption during the manufacturing process. However, the water-based synthesis environment can lead to the incorporation of crystal water within the PB/PBAs structure, which may result in structural instability and undesirable side reactions with organic electrolytes. The presence of crystal water can cause irreversible capacity loss, structural deformation, and gas release during the initial cycling stages due to water decomposition. The presence of crystal water thus leads to performance degradation in the early cycles and negatively impacts both the long-term safety and cycle life of the battery. Therefore, controlling crystal water is critical for optimizing the use of PB as a cathode material of SIBs. Various strategies have been reported on controlling crystal water in PB, including the use of chelating agents, non-aqueous solvents, and high-temperature heat treatments. Among these, high-temperature heat treatment is widely regarded as the most effective method for completely removing crystal water. Previous studies have shown that the removal of crystal water results in the formation of a trigonal phase, which exhibits different reversible charge-discharge behavior compared to water-containing PB, such as activating low-spin Fe sites thereby significantly increasing capacity utilization. Although previous literature has not extensively discussed this, we aim to tackle the critical issues associated with the high-temperature heat treatment method. During high-temperature heat treatment, the removal of crystal water leads to the formation of strong Fe-O bond signals on the surface, which are thought to result from the interaction between Fe ions and water released from the structure. The major issue is the thermodynamic instability of Fe(OH)₃. This instability makes it difficult to obtain reliable and uniform data during electrode fabrication and, upon exposure to moisture, leads to the rapid decomposition of the surface into α-Fe₂O₃ or α-FeOOH (Iron oxide). The formation of these Fe-O bonds and iron oxides can lead to increased gas release containing oxygen during charge-discharge cycles. This may result in structural damage to the electrodes and pose a significant safety risk to the battery. Therefore, there is an urgent need for a new approach that minimizes Fe-O bond formation on the surface while effectively removing crystal water. In this study, we developed a liquid-phase process designed to suppress the accelerated formation of Fe-O bonds that occurs during high-temperature heat treatment. Thermogravimetric analysis (TGA) and X-ray photoelectron spectroscopy (XPS) confirmed that crystal water was removed while Fe-O bond formation was suppressed in this liquid-phase environment. This liquid-phase process, which removes crystal water at lower temperatures, offers a promising alternative to the conventional, energy-intensive high-temperature heat treatment process. Figure 1