Hongbo Tan,Maogao Li,Xingyang He,Ying Su,Jin Guo Yang,Huang Zhao
标识
DOI:10.1016/j.conbuildmat.2020.120465
摘要
As a by-products of lithium carbonate industry, emission of lithium slag (LS) was increasingly increased due to the huge market demand of lithium salt. Therefore, LS disposal faces great challenge. In the study, a new approach to use LS in sulphoaluminate cement (SAC) system to improve the early compressive strength was proposed. Nano-lithium slag (nano-LS) was prepared via wet grinding, and the effect of nano-LS on hydration mechanism of SAC was investigated. The results indicated that nano-LS with D50 of 300 nm was prepared. In comparison with the Blank, 4.0% nano-LS promoted the 7 h compressive strength from 4.5 MPa to 24.3 MPa, with an increase by more than 4 times, and an increase by 28% at 1 d age; it also reduced the initial and final setting time to 16 min and 23 min, being reduced by 33.3% and 37.5%. This phenomenon was because nano-LS accelerated the hydration of SAC, and 4.0% dosage even made the inducing period disappear. The reason for the accelerated hydration was that the nano particles in nano-LS slurry acted as excellent nucleation seeds for speeding of the formation of hydration products. Additionally, the promoted dissolution of lithium salt during the process of wet milling also facilitated precipitation of aluminum phase to accelerate the SAC hydration. Consequently, nano-LS was expected as an excellent accelerator in SAC system. All of findings suggested an innovation new way to utilize LS in SAC system.
科研通智能强力驱动
Strongly Powered by AbleSci AI