Interface Stabilization as a Pathway to Fast Charging Graphite//NCM811 Lithium-Ion Battery
作者
Gwangyong Ko,Jiin Lee,Kihun An,Dung Tien Tuan Vu,Seung‐Wan Song
出处
期刊:Meeting abstracts [Institute of Physics] 日期:2026-07-07卷期号:MA2026-01 (3): 435-435
标识
DOI:10.1149/ma2026-013435mtgabs
摘要
Fast charging of Li-ion batteries (LIBs) with graphite anode is highly desirable for applications such as electric vehicles. However, under fast charging rates, intrinsically sluggish Li-ion intercalation kinetics and non-uniform and unstable solid electrolyte interphase (SEI) layer of graphite anode lead to Li dendrites formation and growth. Dendrites can penetrate soft separator, causing performance failure and internal short-circuits followed by thermal runaway. Herein, we present improved fast charging performance enabled by a designed electrolyte formulation that stabilizes the SEI layer of graphite anode, compared to conventional rate of 0.3C taking 3.3hours, and enhanced cycle life of high-nickel-based LIBs. The correlation between fast charging performance and interfacial stability will be discussed.