摘要
Laser slicing produces wafers from hard and brittle materials, including single-crystal diamond. Scaling this process to millimeter-scale diamond substrates and evaluating the laser-induced damage are important steps toward practical applications. This study investigated the crack-connection conditions for scaling {100}-plane diamond slices and evaluated the damaged-layer depth. During laser slicing, cracks connect adjacent modified regions, forming a continuously modified layer. Increasing the pulse energy and number of laser pulses enlarged the modified regions and increased the magnitude and spatial extent of the measured retardation associated with stress-induced birefringence. Larger modified regions were associated with crack connections over larger intervals between adjacent modified regions. Across the investigated laser conditions, both the minimum and maximum applicable intervals increased with the modified-region volume; therefore, this volume serves as an empirical predictor of the applicable interval range. However, a practical trade-off was observed: smaller modified regions reduced the polishing depth required to remove the damaged layer but made crack connections more sensitive to slight variations in the processing conditions. Consequently, excessively small modified regions reduced the reproducibility of crack connections. The appropriate interval also increased with the modified-layer size, whereas in situ observations suggested that the accumulated elastic strain energy promoted crack propagation. Based on these results, slicing a 3-mm-square diamond substrate was demonstrated. Raman analysis showed that the degraded crystallinity region extended approximately 40 μm from the sliced surface. Polishing the damaged layer restored the Raman peak width to a value comparable to that of pristine diamond. The total material loss was approximately 80 μm. These results provide processing guidelines for millimeter-scale {100}-plane diamond laser slicing and damaged-layer removal.
科研通智能强力驱动
Strongly Powered by AbleSci AI