Twip公司
材料科学
极限抗拉强度
微观结构
锯齿状
冶金
延展性(地球科学)
位错
复合材料
变形(气象学)
可塑性
晶体孪晶
蠕动
作者
Youyun Chen,Wengang Zhai,Juhua Liang,Modi Zhao,Fusheng Han
标识
DOI:10.1016/j.jmrt.2024.06.192
摘要
Twinning induced plasticity (TWIP) high manganese steel exhibits high ultimate tensile strength (UTS) and ductility, but its low yield strength restricts its applications. This research presents a Fe–21Mn-0.6C TWIP steel with enhanced mechanical properties additively manufactured using laser powder bed fusion (LPBF). The average grain size of the LPBF-fabricated Fe–21Mn-0.6C was 17.1 μm in the vertical direction, which was a quarter of that of a wrought one. The tensile yield strength was 657 MPa and the UTS was 1089 MPa with an elongation of 47.9% for the vertical direction. Compared to the wrought Fe–21Mn-0.6C, the yield strength increased by 110%. The high strength of LPBF-fabricated Fe–21Mn-0.6C is primarily attributed to solution, grain boundary and dislocation strengthening. Serrations were observed in the stress-strain curves at the initial stage of deformation, showing large stress drops. In the annealed sample, serrations appeared at a later stage of deformation with little stress drops. This difference in serration phenomenon is attributed to the varying dislocation density in the two samples.
科研通智能强力驱动
Strongly Powered by AbleSci AI