Improvement of a Capacity Utilization By Introducing an Asymmetric Anolyte/Catholyte Volume in Vanadium Redox Flow Battery
作者
Jong‐Ho Park,Jung Hoon Yang
出处
期刊:Meeting abstracts [Institute of Physics] 日期:2016-09-01卷期号:MA2016-02 (5): 844-844被引量:1
标识
DOI:10.1149/ma2016-02/5/844
摘要
As large-capacity energy-storage systems, redox flow batteries have received considerable attention because they can effectively decouple the power density and energy capacity. The power density is determined by the battery stack design while the energy capacity is affected by the amount of redox species dissolved in the electrolyte, which is circulated through the stack and stored in the external reservoirs. The crossover of the redox species between the anolyte and catholyte within the stack causes the self-discharge and decreases the energy capacity. Vanadium redox flow battery employs the same vanadium ions as the redox species in both anolyte (V2+/V3+) and catholyte (V4+/V5+). Therefore, it can partially solve the crossover problem only by remixing and separating the anolyte and catholyte. However, the frequent remixing reduces the system efficiency significantly. Furthermore, the different transfer rates of each vanadium ions through membrane accelerate the crossover, thus resulting in the capacity decay. The diffusion coefficients were in the order of V2+ > V4+ > V5+ > V3+ across Nafion 115 membrane. Minimizing the capacity decay is very important to improve the real energy density of the flow battery. We have observed an interesting point in the relation between the capacity decay and initial volume ratio of the anolyte and catholyte. At a constant volume of the catholyte, the capacity decaying rate was independent of the anolyte volume. On the other hand, the capacity decay was improved with the decreasing volume of the catholyte at a constant anolyte volume. In this study, we have investigated the dependency of the capacity decay on the initial volume ratio of the anolyte and catholyte.