摘要
The lifetime of hydroxyl radicals (⋅OH) in the fuel cell catalyst layer remains uncertain, which hampers the comprehension of radical-induced degradation mechanisms and the development of longevity strategies for proton-exchange membrane fuel cells (PEMFCs). In this study, we have precisely determined that the lifetime of ⋅OH radicals can extend up to several seconds in realistic fuel cell catalyst layers. This finding reveals that ⋅OH radicals are capable of carrying out long-range attacks spanning at least a few centimeters during PEMFCs operation. Such insights hold great potential for enhancing our understanding of radical-mediated fuel cell degradation processes and promoting the development of durable fuel cell devices.
科研通智能强力驱动
Strongly Powered by AbleSci AI