L. A. Davis,P. Ramkumar
标识
DOI:10.1177/13506501221144699
摘要
Premature bearing failures commonly occur in applications that operate under extreme boundary conditions. The lubrication engineers and tribologists are confronting a key challenge in these bearing failures associated with microstructure decay, such as White Etching Cracks (WECs) and White Etching Areas (WEAs). Lubricant degradation is one of the critical factors for the subsurface decay in the bearing steel. This work evaluates the performance of mineral oil (heavy paraffin oil) and synthetic poly alkyl glycol (PAG) against WEAs formation under pure sliding with cyclic compressive loading. The performance of lubricants was evaluated using Infrared Fourier Transform (FTIR) and Electron Spin Resonance (ESR) spectroscopy. The outcomes reveal that the free radical formation rate is higher for paraffin than PAG. This study found that WEAs formation in the bearing steel is delayed in the PAG tested samples compared to paraffin.
科研通智能强力驱动
Strongly Powered by AbleSci AI