摘要
ABSTRACT Near‐infrared‐emitting copper‐based I‐III‐VI quantum dots (QDs) hold significant promise for photonics and bioapplications, yet their broad photoluminescence (PL) emission severely limits color purity and device efficiency. Herein, we report a hierarchically staged synthesis that decouples and sequentially suppresses defect‐ and phonon‐induced broadening. Starting with Zn‐poor CuInSe 2 QDs via cation exchange, we introduce Zn 2+ alloying to passivate cation vacancies and homogenize composition, forming a defect‐minimized core. Subsequent epitaxial overcoating with a thick ZnS shell strongly localizes excitons, evidenced by suppressed thermal quenching and dominant coupling to a higher‐order longitudinal optical ( LO ) phonon mode of ZnS ( E LO ≈ 141 meV). This shifts recombination from defect‐assisted to near‐band‐edge emission, yielding CuInZnSe/ZnS QDs with an ultranarrow linewidth of 111 meV, high PL quantum yield of 73%, and minimal Stokes shift of 42 meV at 977 nm. When integrated into luminescent solar concentrators, these QDs enable an optical efficiency of 8.81% and a power conversion efficiency of 2.79%, underscoring their practical utility. Beyond reporting materials, this work provides profound insights into the interplay of exciton confinement and defect engineering, establishing a general and instructive strategy for achieving high color purity in multinary QDs.
科研通智能强力驱动
Strongly Powered by AbleSci AI