Qingan Zhang,Miaohui Fang,Tingzhi Si,Fang Fang,Dalin Sun,Liuzhang Ouyang,Min Hua Zhu
摘要
The phase stability, structural transition, and hydrogen storage characteristics of the polymorphic La 4 MgNi 19 compound are systematically investigated in the present work. The La 4 MgNi 19 compound has two variants in the temperature range of 840−960 °C with a preference for a hexagonal structure (2H) at a higher temperature and a rhombohedral structure (3R) at a lower temperature. Because the structure and composition are almost identical, the polymorphic transition between the 2H and 3R phases may proceed through short-range displacements of their subunit layers. Detailed analyses on XRD patterns for the hydrided or dehydrided samples indicate that the equilibrium pressures of hydrogen absorption and desorption for the 2H phase are lower than the pressures for the 3R phase, but the pressure gap between the two phases is too small to be identified from the measured pressure−composition ( P − C ) isotherms. The average hydriding and dehydriding enthalpies are determined to be −32.1 and 31.5 kJ/mol H 2, respectively. As hydrogen atoms enter into the lattices, the strains in both the 2H and the 3R phases increase first in the region of the dilute H-dissolved solid solutions and then dramatically decrease once the dilute solid solutions transform into the corresponding hydrides.
科研通智能强力驱动
Strongly Powered by AbleSci AI