催化作用
X射线光电子能谱
纳米颗粒
多相催化
化学工程
钙钛矿(结构)
材料科学
热稳定性
多孔性
热处理
催化燃烧
无机化学
化学
复合材料
有机化学
工程类
作者
Lei Li,Jinlong Yan,Weijie Ji
标识
DOI:10.1016/j.apcata.2022.118947
摘要
Tuning the microenvironment of noble-based catalyst is a key issue for improved catalytic performance. Here, the porous MnO x enclosed Pd nanoparticles were successfully fabricated by template-free method, that was based on an acid-etching strategy using Pd-doped manganite perovskite (e.g., LaPd 0.1 Mn 0.9 O 3 ) as precursor. The performance of prepared Pd/MnO x catalyst is beyond the performance of acid-treated MnO 2 and traditional Pd/MnO 2 catalyst, showing a T 90 of 200 o C under a space velocity of 60,000 mL/(g.h). The superior performance should be attributed to the exposure of Pd active sites, the large surface area, abundant oxygen vacancies and the synergistic effect between Pd and MnO x support. XPS spectra demonstrated that the change of Pd oxidation state was well associated with catalytic activity, and the mixed Pd 0 /Pd n+ species were benefit for improved activity. On the basis of in-situ XRD and TG results, it was revealed that the thermal deactivation was caused mainly by the structural change of MnO x other than the Pd oxidation state. And the structural stability could be strengthened by the thermal treatment at high temperature (e.g., 500 o C), and remained a robust performance over the long-term stability test. • Porous MnO x enclosed Pd nanoparticles were successfully fabricated via an acid etching strategy. • The formed Pd/MnO x catalyst shows a superior performance (T 90 = 200 °C). • High exposure of Pd active-sites, large surface area and rich oxygen vacancies contributes to superior activity. • Structural evolution of MnO x matrix results in thermal deactivation other than the Pd oxidation state.
科研通智能强力驱动
Strongly Powered by AbleSci AI