材料科学
焊接
脆性
合金
冶金
低温
转变温度
复合材料
凝聚态物理
超导电性
物理
作者
Shengli Li,Chunjin Hang,Qilong Guan,Xiaojiu Tang,Ning Zhou,Yanhong Tian,Wei Zhang,Dan Yu,Ying Ding,Xiuli Wang
标识
DOI:10.1016/s1003-6326(24)66748-8
摘要
The inherent brittle behavior and ductile-to-brittle transition (DBT) mechanism of Sn−3.0Ag−0.5Cu (SAC305) solder alloy at the liquid nitrogen temperature (LNT, 77 K) were investigated through uniaxial tensile experiments conducted at different temperatures. Dynamic recovery and recrystallization of SAC305 solder alloy at room temperature (RT, 293 K) activate a softening process. Conversely, intersecting and none-intersecting deformation twins, embedded in body-centered tetragonal Sn, enhance tensile strength and stabilize strain hardening rate, while suppressing the elongation of the alloy at LNT. The irreconcilable velocity difference between twin thickening (~8 µm/s) and dislocation slip (~4 µm/s) results in premature brittle fracture, during the linear hardening and DBT. Moreover, the secondary phases degrade the mechanical property of SAC305 solder alloy, and micro-cracks appear between Cu 6 Sn 5 and Ag 3 Sn in the eutectic matrix.
科研通智能强力驱动
Strongly Powered by AbleSci AI