Hanyang Xu,Yuankui Sun,Jinxiang Li,Feng‐Min Li,Xiaohong Guan
标识
DOI:10.1021/acs.est.6b01763
摘要
Scanning electron microscopy (SEM), Raman spectroscopy, and X-ray photoelectron spectroscopy (XPS) depth profiling were employed to characterize the aged zerovalent iron (AZVI) samples incubated in synthetic groundwater. The AZVI samples prepared under different conditions exhibited the passive layers of different morphologies, amounts, and constituents. Owing to the accumulation of iron oxides on their surface, all the prepared AZVI samples were much less reactive than the pristine ZVI for Se(IV) removal. However, the reactivity of all AZVI samples toward Se(IV) sequestration could be significantly enhanced by applying a uniform magnetic field (UMF). Moreover, the flux intensity of UMF necessary to depassivate an AZVI sample was strongly dependent on the properties of its passive layer. The UMF of 1 mT was strong enough to restore the reactivity of the AZVI samples with Fe3O4 as the major constituent of the passive film or with a thin layer of α-Fe2O3 and γ-FeOOH in the external passive film. The flux intensity of UMF necessary to depassivate the AZVI samples would increase to 2 mT or even 5 mT if the AZVI samples were covered with passive films being thicker, denser, and contained more γ-FeOOH and α-Fe2O3. Furthermore, increasing the flux intensity of UMF facilitated the reduction of Se(IV) to Se(0) by AZVI samples.
科研通智能强力驱动
Strongly Powered by AbleSci AI