材料科学
微观结构
各向同性腐蚀
蚀刻(微加工)
退火(玻璃)
X射线光电子能谱
复合材料
溅射
溅射沉积
干法蚀刻
硅
薄板电阻
冶金
反应离子刻蚀
等离子体刻蚀
薄膜
微电子机械系统
光电子学
纳米技术
半导体
矿物学
形成气体
作者
Shiao Wang,Q. Fu,Hongyang Zhao,Tomasz W. Liskiewicz,Ben D. Beake
标识
DOI:10.1016/j.surfcoat.2025.133040
摘要
Y 2 O 3 films with enhanced etching resistance were fabricated on silicon substrates using RF magnetron sputtering followed by vacuum annealing at 300 °C, 600 °C, and 900 °C. The films were systematically evaluated under chemical, mixed, and physical plasma etching environments using CF 4 /Ar/O 2 gas mixtures. Annealing at 900 °C transformed the microstructure from quasi-circular grains to densely packed polygonal grains with layered stacking, significantly improving the structural compactness of film. Y 2 O 3 films demonstrated superior etching resistance compared to conventional materials including Al 2 O 3 , SiC, AlN, and quartz. The 900 °C-annealed film under vacuum showed highest resistance under chemical and mixed etching, while the 600 °C-annealed film under vacuum performed best under physical etching due to superior hardness (7.2 ± 2.0 GPa). Nanomechanical testing revealed that physical etching resistance correlates with hardness, while chemical and mixed etching resistance depends on the structural compactness of film. Nano-indentation and nano-scratch testing showed that coatings annealed in air were softer and less scratch-resistant than those annealed in vacuum, with differences being more pronounced in statistically distributed nano-scratch testing. X-ray photoelectron spectroscopy confirmed distinct mechanisms: chemical etching involves protective Y F bond formation, mixed etching shows enhanced Y F stability, and physical etching induces oxygen vacancies. This study establishes a cost-effective strategy for enhancing etching resistance through microstructural optimization, offering promising implications for semiconductor manufacturing applications.
科研通智能强力驱动
Strongly Powered by AbleSci AI