Mahdi Mashkour,Yahya Ranjbar
标识
DOI:10.1016/j.indcrop.2017.09.068
摘要
Abstract Given the high potential applications of magnetic green polymer nanocomposites in the construction, automotive and military industries, fabrication and characterization of superparamagnetic Fe3O4@ wood flour/polypropylene nanocomposites were investigated for the first time in this study. Magnetite (Fe3O4) nanoparticles were in situ synthesized on poplar wood flours. The filler loading used was 40 wt.% and the virgin wood flours (VWFs) and magnetic wood flours (MWFs) were used as filler at three levels of mixing ratios (VWFs: MWFs = 100:0, 50:50, and 0:100 wt.%). Maleic anhydride-grafted PP (MAPP) was used as the MAPP at two levels of 1 and 3 wt.%. Characterization of the MWFs confirmed the successful “in situ synthesis” of spherical superparamagnetic Fe3O4 nanoparticles on the wood flours with an average crystal size of about 8 nm at approximately 30 wt.%. The physical properties examinations indicated that the increase of MWFs up to 100 wt.% of filler phase increased the long-term water absorption and thickness swelling of specimens up to 2.6 and 2.4-fold, respectively. The ultimate tensile and flexural strengths increased when MWFs increased by up to 50 wt.% and then decreased at higher weight ratios of MWFs. Increasing the MAPP from 1 to 3 wt.% improved both physical and mechanical properties, but this effect was more perceptible in improving mechanical strengths compared to the elastic modulus. The magnetization characterization showed about 10% reduction in saturation magnetization (Ms) of the final MWFs/polypropylene nanocomposites in comparison with the Ms values of the starting MWFs (≈1 emu/g). This observation was attributed to the formation of a nonmagnetic layer on the Fe3O4 nanoparticles during the melt-blending process.
科研通智能强力驱动
Strongly Powered by AbleSci AI