A nickel-base superalloy has been used to deposit the aluminide coating by low-temperature pack cementation process. The high temperature oxidation tests on aluminized alloys and the uncoated specimens are carried out at 1000°C for 10h. It is observed that a dense and protective Al 2 O 3 surface layer is produced on the aluminized alloy, and the aluminizing process has greatly enhanced the high temperature oxidation resistance of the Ni -base superalloy at 1000°C. As a contrast, the uncoated specimen begins to be failure when treated only for 6h at the same temperature.