Jin Zhang,Yanfei Wang,Xiangjian Chen,Yanzi Gou,D Y Li,Rongjun Liu
摘要
ABSTRACT SiC f /SiC composites were fabricated using two categories of third‐generation SiC fibers: S‐type (smaller grains, higher strength) and SA‐type (larger grains, lower strength), followed by 100‐h heat treatment at 1500°C in argon. The results indicate that the crystallization of amorphous SiC x O y phase in Cansas‐III fibers (S‐type) causes fiber volume shrinkage, leading to large‐area debonding between PyC and fibers. While the sublimation of Si in KD‐SA fibers (SA‐type) migrates into the PyC interfacial layer and reacts with PyC to form SiC, resulting in discontinuous SiC particle bands in the central region of PyC interfacial layer. KD‐SA SiC f /SiC composites exhibit higher initial IFSS due to a highly rough fiber surface. After 100 h of heat treatment, the IFSS of KD‐SA SiC f /SiC composites remains at a high level of approximately 150 MPa due to the enhanced friction caused by SiC particle bands. While the IFSS of Cansas‐III SiC f /SiC composites decreases from 64.17 to 51.73 MPa.
科研通智能强力驱动
Strongly Powered by AbleSci AI